TítuloLow temperature solid state processing of pure P3HT fibers
Autor(es)Rodrigues, Alexandre
Nabankur, Deb
Hilliou, L.
Viana, J. C.
Bucknall, David G.
Bernardo, Gabriel
Palavras-chaveP3HT
Processing
Solid state
Conductive polymer
Data2013
EditoraAIP Publishing
RevistaAIP Advances
Resumo(s)Fibers of pure poly(3-hexylthiophene) (P3HT) of 1 and 2mmdiameter, were produced from solid state processing at temperatures of 200, 150 and 100oC, i.e. up tomore than 100 oC below the melting point of P3HT (∼240 oC), using a small device reminiscent with the early stage polymer extrusion machines. The fibers produced by this method are continuous and mechanically robust.WAXS results showthat themacromolecular chains of P3HT are preferably oriented along the fiber axis. This study clearly shows, for the first time, that P3HT fibers can be processed without solvents well below the polymer’s melting temperature.
TipoArtigo
URIhttps://hdl.handle.net/1822/24104
DOI10.1063/1.4806764
ISSN2158-3226
Versão da editorahttp://aipadvances.aip.org/resource/1/aaidbi/v3/i5/p052116_s1
Arbitragem científicayes
AcessoAcesso restrito UMinho
Aparece nas coleções:IPC - Outras publicações/Other publications

Ficheiros deste registo:
Ficheiro Descrição TamanhoFormato 
AIP advances 2013.pdf
Acesso restrito!
author copy1,6 MBAdobe PDFVer/Abrir

Partilhe no FacebookPartilhe no TwitterPartilhe no DeliciousPartilhe no LinkedInPartilhe no DiggAdicionar ao Google BookmarksPartilhe no MySpacePartilhe no Orkut
Exporte no formato BibTex mendeley Exporte no formato Endnote Adicione ao seu ORCID